Data from: A Ni(II) PNP pincer complex immobilized on SBA-15 as catalyst for the 4-nitrophenol hydrogenation

Data files

Jul 09, 2026 version files 1.21 MB

Click names to download individual files

Abstract

The Ni(II) complex [NiCl(bda)]+ containing the aliphatic PNP pincer ligand bis((2-diphenylphosphino)ethyl)amine (bda) was covalently immobilized on the mesoporous silica SBA-15. SBA-15 was functionalized with (3-chloropropyl)triethoxysilane (CPTES) as an anchoring agent, which was further reacted with the amine group of the Ni-coordinated bda ligand forming the hybrid material SBA-15@PTES@Ni. The material was characterized using Fourier-transform infrared spectroscopy (FT-IR), UV-vis-DRS (diffuse reflectance) spectroscopy, thermogravimetric analysis (TGA), low angle X-ray diffraction (la-XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and energy dispersive X-ray spectroscopy (EDS), and inductivity coupled plasma (ICP-AES). SBA-15@PTES@Ni was used as a catalyst for the hydrogenation of 4-nitrophenol (4-NP) to 4-aminophenol (4-AP) using NaBH4 in aqueous solution. With catalyst loadings of 1 to 3 mg, complete conversions were achieved in 6 to 10 min, with rate constants up to 6.92 ×10–3 s–1.